MER Group gaw, laksan hkrang shapraw ai lam, jak rung galaw ai lam, n-gun dat ai lam, wan wut hpaw hpang ai lam hte bungli galaw ai lam ni hpe gram lajang ai lam ni hpe hpawng de da ai hpaji rawng ai mungdan kata na hpaga hpung langai mi re. Ya aten du hkra, anhte gaw n-gun n-gun hpe hkye la ai rotary‐kiln active‐lime masing amyu myu 200 daram hpe galaw lai wa sai.
Hpaga lam hpe tsun dan ai
Dai majaw, n-gun ja ai n-gun hpe jai lang ai rotary kiln active‐lime (burnt lime) galaw shapraw ai ladat gaw, preheater, rotary kiln hte vertical cooler ni lawm ai kungkyang ai ladat hpe hkap la ai. Ndai hpaji masa gaw n-gun lang ai lam hpe shayawm ya ai, shapraw ai lam hpe jat ya ai hte bungli galaw ai manu hpe shayawm ya ai sha n-ga, n-gun n-gun hpe hkye la ai hte n-gun dat hpe shayawm ya ai hta laklai ai bungli ni hpe galaw ya lu ai. Dai gaw, active burnt lime hpe langai sha re ai hku n-gun dat na matu, manu dan dik ai ladat ni hte arung arai ni hta lawm nga ai.
Anhte a rotary lime kiln gaw, n-gun ja ai wan sau hpe wan nat ai hpaji masa hpe gumrawng nga ai. Shi gaw n-gun hpe atsawm sha makawp maga lu na matu fine‐grained wan sau hte low‐calorific‐value wan sau hpe madi shadaw ya ai. Container‐style modular gawgap ai lam gaw, shata sanit laman bungli masing hpe ngut kre hkra galaw lu nna, bungli galaw hpang lu ai. Hpang jahtum galaw ngut sai bungli masing lahkawng tsa kaw na grau kaja hkra galaw ai Civil‐engineering masing ni gaw, client ni hpe capital gawgap ai manu hpe 20% shayawm ya lu ai. Ndai jak gaw 10%‐20% over‐production margin hpe galai shai mai ai atsam a matu tawn da ya ai, manu jahpu hpe shayawm ya ai, gawgap ai aten kadun ai hte hkai lu hkai sha ai lam hta hkum tsup ai akyu ni hpe la sa ya ai.
MER Group preheater gaw grau kaja ai nbung‐galai shai ai atsam hpe jaw ya ai. Limestone gaw rotary kiln kata kaw n-gun n rawng shi yang, pre‐heating hte daw mi hten za mat ai hpe hkrum sha ra ai. Flue‐gas waste heat hpe hkum tsup hkra bai jai lang nna galaw shapraw ai atsam hpe jat wa shangun ai. Anhte a mungdan kata na hpaji ningnan ni hpe gram lajang mai ai preheater a matu gaw, hkap la mai ai particle‐size raw materials ni hpe grau dam lada hkra galaw ya ai.
MER Group vertical cooler gaw, n-gun ja ai hte katsi ai hpe pyi galai shai lu na matu, rawt jat galu kaba wa ai uniform cooling‐nbung garan ai hpaji hpe jai lang ai. Katsi ai hpe htawt sit ngut ai hpang katsi ai secondary nbung hpe rotary kiln de hkrak sha bai nhtang bang ai.
Tinang hkum tinang galaw shapraw ai n-gun n-gun n-rawng ai lung seng ni hpe rotary‐kiln lining hta bang da ai. Dai majaw, n-gun ja ai wan n-ga ni hte shingdaw yang, shell‐surface temperature hpe grai shayawm ya nna, kiln‐lining a prat hpe galu shangun ai.
Hpaji masa lam ni hpe hkrak tup tsun dan ai
(1) Raw‐material n-gun n-gun: 10‐60 mm
(2) Jai lang mai ai wan sau ni: n-gun ja ai wan sau hpe galai shai lu ai gaseous, solid, liquid hte mixed wan sau ni
(3) Shani shagu shapraw lu ai atsam: lani mi hta ton 100‐1600
(4) Hpang jahtum na‐lime grade: Grade‐1 nlung htu ai lime
Madung jai lang ai ginra ni
Hpri hte n-gang galaw ai bungli, alumina hte magnesia galaw shapraw ai, desulfurizer galaw shapraw ai
Hpaji ladat ni a matu lung seng law law hpe galaw shapraw ai bungli masa ni hte alkaline jat bang ai lam ni
Calcium-carbide tsi hpaji daw